Wafer → cleaning → transparent electrode layer → transparent electrode graphics lithography → corrosion → glue → platform graphics lithography → dry etching → glue → annealing Sio 2 deposition → window graphic lithography Sio 2 corrosion → Shan Polar graphics lithography → pre-cleaning → coating → stripping → annealing Ship polar graphics lithography → coating → stripping → grinding → cutting → chip → finished testing.
In fact, the production process of epitaxial tablets is very complex, after the exhibition of Epitaxial films, the next step is to start on the LED wafer electrode (p pole, n pole), and then began to use laser cutting LED wafer (formerly cutting led wafer mainly with diamond knife), made into a chip, in different positions on the wafer to extract nine points to do the parameter test.
1, mainly on the voltage, wavelength, brightness test, can meet the normal shipping standard parameters of the wafer and then continue to do the next operation, if these nine test does not meet the relevant requirements of wafer, on the side of the other treatment.
2, wafer cut into the chip, 100% of the Eye inspection (Vi Vc), the operator to use a magnification of 30 times times the microscope under the visual.
3, then the use of automatic classification machine based on different voltage, wavelength, brightness of the predictive parameters of the chip to be fully automated selection, testing and classification.
4, the last to the LED chip check (VC) and labeling. Chip area in the center of the blue film, the blue film up to 5000 chips, but must ensure that the number of chips per blue film should not be less than 1000 tablets, chip type, batch number, quantity and photoelectric measurement statistics recorded on the label, attached to the back of the wax light paper. The chip on the blue film will do the final eye test with the same standard for the first time, to ensure that the chip is arranged neatly and the quality is qualified. This makes the LED chip.